Dear all,
In Cold forming Super duplex SS. (Like Zeron etc.) are there specific high pressure lubricants used?
I am thinking that a lube should have C so that you don't impregnate the surface.
Any experiences?
thanks
In Cold forming Super duplex SS. (Like Zeron etc.) are there specific high pressure lubricants used?
I am thinking that a lube should have C so that you don't impregnate the surface.
Any experiences?
thanks