Anyone of you have came across with the following sulphuric acid specifications in the market:
H2SO4 = 98 wt%
Chlorides as Cl = <40 mg/kg
Fe = <50 mg/kg
NO2 = <50 mg/kg
SO2 = <15 mg/kg
As = <0.1 mg/kg
Hg = <0.1 mg/kg