Hello Guys
I need some guidance regarding Super Duplex Forging SA-182 F53 (UNS32750).
We are in process to procure forging to build ASME U-Stamp, High Pressure Filter Vessel. However, we are having issues with this material not meeting Tensile (116 KSI) and Yield (80 Ksi) as required by ASME SA-182 Ed.2019 specification. Forging are almost 9-10" thick and 24 " diameter.
Our supplier is getting Tensile 113 KSi and Yield 77 Ksi. These strength values are acceptable per ASTM A-182 but not per ASME SA-182. Our Supplier has tried re-heat and retest but still no improvement.
Undoubtedly, for ASME U-stamp vessel, all pressure boundary items has to meet "SA" spec.
Now question is;
1. Is there any exception or way we can use this material(ASTM A-182 F53) and still U-Stamp the vessel?
2. Does anyone had an experience with this material and can advise some inputs for forging process itself which can result the required mechanical properties?
Thanks
I need some guidance regarding Super Duplex Forging SA-182 F53 (UNS32750).
We are in process to procure forging to build ASME U-Stamp, High Pressure Filter Vessel. However, we are having issues with this material not meeting Tensile (116 KSI) and Yield (80 Ksi) as required by ASME SA-182 Ed.2019 specification. Forging are almost 9-10" thick and 24 " diameter.
Our supplier is getting Tensile 113 KSi and Yield 77 Ksi. These strength values are acceptable per ASTM A-182 but not per ASME SA-182. Our Supplier has tried re-heat and retest but still no improvement.
Undoubtedly, for ASME U-stamp vessel, all pressure boundary items has to meet "SA" spec.
Now question is;
1. Is there any exception or way we can use this material(ASTM A-182 F53) and still U-Stamp the vessel?
2. Does anyone had an experience with this material and can advise some inputs for forging process itself which can result the required mechanical properties?
Thanks