Oct 12, 2005 #1 MatEngTED Materials Sep 27, 2004 24 US Need to locate supplier source(s) for polyvinyl butyral (PVB) phenolic film. Any recommendations appreciated.
Need to locate supplier source(s) for polyvinyl butyral (PVB) phenolic film. Any recommendations appreciated.
Oct 12, 2005 #2 Demon3 Materials Jun 6, 2005 1,850 US PVB is not a phenolic resin so I am confused about your request. A quick google search shows DuPont and Wacker as PVB producers. They are global so ask them for your local dealer. Upvote 0 Downvote
PVB is not a phenolic resin so I am confused about your request. A quick google search shows DuPont and Wacker as PVB producers. They are global so ask them for your local dealer.
Oct 12, 2005 Thread starter #3 MatEngTED Materials Sep 27, 2004 24 US The phenolic acts as a crosslinking agent. Upvote 0 Downvote
Oct 13, 2005 #4 Demon3 Materials Jun 6, 2005 1,850 US Cool. Didn't know anyone cross-linked that polymer. By the way it's quite expensive stuff the PVB but you can get it used (recycled from cars) cheaply. I have a friend working with that. Upvote 0 Downvote
Cool. Didn't know anyone cross-linked that polymer. By the way it's quite expensive stuff the PVB but you can get it used (recycled from cars) cheaply. I have a friend working with that.