TylerD

Automotive
Jan 17, 2024
2
Currently we are machining parts prior to heat treat, sending them to heat to treat and then to the customer. Am I mistaken but won't my surface finish change after heat treat? Specifically referencing 12L14 Steel. Appreciate any feedback.
 
Replies continue below

Recommended for you

TylerD,

Do you inspect your parts after heat treating?

--
JHG
 
You can specifically state on the drawing that your desired surface finish applies before/after heat treatment.
 
It will change, not sure how much. But, I agree with Wuzhee, add a note on the dwg.

Chris, CSWP
SolidWorks
ctophers home
 
OK thank you! We normally send it to heat treat and then to the customer.
 