Steved
Industrial
- Aug 25, 1999
- 32
Hello:
How are you? I was wondering if anybody is aware of the change in surface finish (Ra and Rz) to an aluminum surface after anodizing? Prior to anodizing, the surface finish will be submicron - will it change after anodizing?
Thank you,
Steve
How are you? I was wondering if anybody is aware of the change in surface finish (Ra and Rz) to an aluminum surface after anodizing? Prior to anodizing, the surface finish will be submicron - will it change after anodizing?
Thank you,
Steve