I need to have a 3/8" round bar finsihed with a surface finsh of 12-16 microinches. Is this something that is going to be achievable using 8620 or 4340 without being heat treated and being ground. The part would be machined on a lathe.

Is there a rule of thumb on what surface finish is possible according to the hardness. Or are the two related?




 
If it's one piece, you might turn it slightly oversize and polish to get the finish. For a production run, I think you'd be better off adding a grinding operation.

Software For Metalworking
 
Hardness and surface finish are not related. Those two alloys can achieve the stated roughness.
 
CoryPad, the surface finish is more related to the material composition rather than hardness, correct?

 
To get that type finish you should start with a clean steel. A common name in the trade is Aircraft Quality especially with the 4000 series materials.

Could you start with a TGP bar like Mirraloy from Associated Steel. We used this material in place of a 4140,4130,3140, along with 4340 on some parts.

 
No, the surface finish is a function of the manufacturing processes.
 