any know the ASME SA number for SIS 2101 or SIS 14 2101. The SS number may also be helpfull
 
Replies continue below

Recommended for you

The suggested Rolled Alloys' paper is the data sheet for a duplex stainless steel, LDX 2101, while SIS 14 21 01 (or rather SS 14 21 01) is the Swedish standard for a carbon-manganese pressure vessel steel. Determining the corresponding ASTM/ASME steel is not easy, since the Swedish standard covers, sheet, plate, bar, and pipe/tube (seamless and welded). You can possisbly get better information from the Swedish Standard Institute,
 