Below is the excerpt from API 5CT (9th edition, latest)
C110 material:
"Particular attention should be given to the application of Grade C110 in ISO 15156-2 or ANSI-NACE MR0175/ISO 15156-2 SSC Regions 2 or 3, as this material is not suitable for all sour (hydrogen sulfide-containing) service applications".
My questions are here
"can C110 material be used for SSC Regions 2 and 3 ?
If not, why API 5CT recommends this material for sour service with NACE TM0177 testing ??
Is C110 listed in NACE MR0175
Regards
Below is the excerpt from API 5CT (9th edition, latest)
C110 material:
"Particular attention should be given to the application of Grade C110 in ISO 15156-2 or ANSI-NACE MR0175/ISO 15156-2 SSC Regions 2 or 3, as this material is not suitable for all sour (hydrogen sulfide-containing) service applications".
My questions are here
"can C110 material be used for SSC Regions 2 and 3 ?
If not, why API 5CT recommends this material for sour service with NACE TM0177 testing ??