rbk1234
Mechanical
- Mar 20, 2016
- 1
Our client want to check their bottom plate . before it was lap joint but now bottom plate has butt joint. The leave their old annular plate as it is,but now they weld bottom plate directly to the shell . the height between existing annular plate and new bottom plate is 1in. is it acceptable or not?