Hi
Recently We have tapping problem in manufacturing component and the details as under one of the component steel material having M30 Nut for that locking screw M5 threading for that we have done drilling 4mm drill then we have done tapping M5 tapping by hand for that we have observed NO GO answering gauge
What could be reason NO GO Answering gauge?
Same process (drill and same tapping) carried out on one dummy plate on that Thread gauge GO answering and it is OK.
Here my question is what could be reason for threading NO GO Answering?
If anybody having in this Please help
Thanks & Regards,
P V K Raju
Recently We have tapping problem in manufacturing component and the details as under one of the component steel material having M30 Nut for that locking screw M5 threading for that we have done drilling 4mm drill then we have done tapping M5 tapping by hand for that we have observed NO GO answering gauge
What could be reason NO GO Answering gauge?
Same process (drill and same tapping) carried out on one dummy plate on that Thread gauge GO answering and it is OK.
Here my question is what could be reason for threading NO GO Answering?
If anybody having in this Please help
Thanks & Regards,
P V K Raju