The Temperature Coefficient for Metal Film Resistors defined by manufacturers as +/- ppm.
What is the reason for such definition (what is the physical process for decreasing resistance with increasing temperature)?
 
Replies continue below

Recommended for you

Podri,
I guess I never paid much attention to MF but should not the resistance go down with a decrease in temp?
 
There are two thermal effects: 1.) the spec. R of the metall
is increasing with T. 2.) The thermal expansion of the substate.


<nbucska@pcperipherals.com>
 