Temperature depence of viscosity of a polymer 1

Status
Not open for further replies.

bauer1989

Industrial
May 22, 2017
1
Hi,

I am working on the temperature dependence of viscosity of a polymer.

I would like to model it on ANSY FLUENT et plot a curve on excel.

My problem is within the Arrhenius law:
nu = K*gamma^(n-1)*exp[alpha(1/(T-To) - 1/(T-Talpha)]
I don't get the difference between temperatures To and Talpha.
It says that the both are reference temperature, but i would to know the difference.


Thanks in advance fro your help.

 
Replies continue below

Recommended for you

To model viscosity change with temperature you must know the value of viscosity at two different temperatures.
So, I would think that there are two reference viscosities (two values) which are each given at their respective reference temperature, To and Ta.

Technology is stealing American jobs. Stop H1-Bs for robots.
 
jari, Thanks (*). I learned something from that.

Technology is stealing American jobs. Stop H1-Bs for robots.
 
Glad to be of some help =)
Hopefully, the OP learned what they were looking for too!
 
Never know. You can lead a horse to water, but you can't make them drink.

Technology is stealing American jobs. Stop visas for robots.
 
The last time I got tangled up in a similar situation with bitumen, none of the equations I could get my hands on would cover the entire temperature range with reasonable accuracy. I had to derive a polynomial expression myself, and also break up the curve into 3 temperature ranges, with a different polynomial expression for each range. Things get a little easier when you have Mathcad to help.
 
I normally use the Andrade equation, but my typ fluids are the more conventional oils and petro products. I thought it could have been similar to that.

Technology is stealing American jobs. Stop visas for robots.
 