padovano

Petroleum
Dec 13, 2006
73
our catalytic reforming unit is made up of 4 furnaces and 4 reactors(IFP). The temperature difference across the 3rd reactor was designed to be between 40 and 50 degrees. But for more than 6 months now the temperature difference is between 15 to 25 degrees.The pressure is ok. This is the only reactor given a temperature difference out of its designed specification. Can somebody surgest to me what might be the possible cause of this temperature gradient.
 
Replies continue below

Recommended for you

padovano, just for our understanding, is this a unit that is only 6 months old or has the delta T changed vs 6 months ago (which would be strange)?
 

The best answer should be provided by IFP themselves.

Anyway, as I figure it, the general multireactor CCR approach includes the following reactions:

[•] In the first reactor the prime reaction is naphthene dehydrogenation (endothermic: ~51-53 kcal/g mole)

[•] In the second reactor, further dehydrogenation and some paraffin dehydrocyclization (endothermic: ~11-17 kcal/g mole) take place with a further drop in temperature

[•] In the third and fourth reactors, slower paraffin isomerization (exothermic:~2.3 kcal/g mol) and paraffin hydrocracking (exothermic:~13.5 kcal/g mole) start to predominate.

Thus, temperature drops in each reactor would normally be affected by a balance among the various reactions, which themselves can be affected by the type of feedstock.
 
the delta T changed just six months ago.
 