Test pressure standard

Status
Not open for further replies.

ajraorane

Mechanical
Sep 16, 2014
1
If any one help me for Test pressure standard of ASTM A671 Gr. CB60 CL12 EFW pipe?
 
Replies continue below

Recommended for you

For class 12, refer to A671 para 1.3.3 (I have the 2004 edt in front of me), which refers to para 8.3 of A671, which refers to ASTM A530 section 6.

Do you own a copy of the relevant ASTM standard(s)?
 