Quality2479
Materials
We are reviewing most of the Electrode/Filler Wire batch test certificates of various reputed welding consumables manufacturers and noted that only Chemical analysis is actual analyzed and mentioned in the Test certificate and whereas for Mechanical Properties only typical values are mentioned as per ASME Sec. II Part-C which are not actual results.
For Example - For GTAW wires-As per ASME Sec. II Part-C SFA 5.18 Table-5, Tension test is required for ER70S-2 filler wire, but we are recieving the batch test certificates without Mechanical properties.
Question-Is Actual Mechanical tests for Welding consumables non-mandatory?
Thanks in advance for reply.