I am preparing the method statement of precast concrete manholes , what are the tests we have to do for the manholes before the backfilling.
Thanks
 
Replies continue below

Recommended for you

make sure the lifting holes are plugged. If there is ground water, gaskets between each section. Plumb and level. Manhole castings are sealed to barrel. Do not allow the roadwork guys to reset the castings without your inspection. Some peol=ple like to match the road surface with the castings by using non-standard methods, ie rocks wooden wedge.