Thanks Bill,

Your information is definitely helpful. The process is co-extrusion of Polypropylene/Polyethylene/Polypropylene for a trilayer battery seperator used in high energy rechargeable Li-batteries.

The resins are isotactic Polypropylene and Highdensity polypropylene.

Can you give me some startup information on the cost estimation of site prep, foundations, steel work, piping, electrical and anxillary systems and controls...I appreciate if you can direct me to useful resources...

Velugula
 