Oct 26, 2016 #1 Pipoy04 Mechanical Nov 22, 2014 40 0 0 QA Dear Experts, I would like to know if there's acceptance criteria for the TBC spallation of gas turbine blades? Is there any reference codes or standards?
Dear Experts, I would like to know if there's acceptance criteria for the TBC spallation of gas turbine blades? Is there any reference codes or standards?
Oct 28, 2016 #2 metengr Materials Oct 2, 2003 15,478 0 0 US Usually this falls under the turbine OEM for guidance. Upvote 0 Downvote
Nov 5, 2016 #3 racookpe1978 Nuclear Feb 1, 2007 5,968 0 36 US And your OEM really, really, really does NOT want you allowing ANYBODY else to analyze his turbine blade and vane designs, ceramics, cooling air flow, and - most espcially - any problems you (and he) may be having with his blade and vane designs! Upvote 0 Downvote
And your OEM really, really, really does NOT want you allowing ANYBODY else to analyze his turbine blade and vane designs, ceramics, cooling air flow, and - most espcially - any problems you (and he) may be having with his blade and vane designs!