Thermal shrink fitting contact problem
Hallo
I am doing 2D shrink fitting contact analysis. The shaft material is 42CrMo4 and the hub material is 20Mn5.
the temperature of the shaft (inner part)is 20 C and the temperature of the hub (Outer part) is 170 C. there is a gap of 1.1 mm in between.
the hub (Outer part)is allowed to cool for 50000 sec to get shrink fitted to the shaft(inner part).
I want to calculate the contact pressure and the stresses in both shaft and hub material(Contact analysis)
Problem
I am confused in the options to be given to the contact and target elements in the contact analysis.
Does anybody have sample problem solution or macro for 2D thermal shrink fit contact analysis problem ??
Amol
Hallo
I am doing 2D shrink fitting contact analysis. The shaft material is 42CrMo4 and the hub material is 20Mn5.
the temperature of the shaft (inner part)is 20 C and the temperature of the hub (Outer part) is 170 C. there is a gap of 1.1 mm in between.
the hub (Outer part)is allowed to cool for 50000 sec to get shrink fitted to the shaft(inner part).
I want to calculate the contact pressure and the stresses in both shaft and hub material(Contact analysis)
Problem
I am confused in the options to be given to the contact and target elements in the contact analysis.
Does anybody have sample problem solution or macro for 2D thermal shrink fit contact analysis problem ??