Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Thermal spraying over martensitic stainless steel

Status
Not open for further replies.

DesignerKPB

Mechanical
Joined
May 8, 2002
Messages
3
Location
US
Hi,

We are thinking in applying a Metco 18C linning to a 1.4418 substract. The problem is:
The substract is quenched and tempered (1200°C and 550°C respectively).
The Metco 18C powder needs to be heated to 1100°C and cooled slowly.
It will change the original martensitic structure (80% matensite - 15% austenite - 5% ferrite)to another structure, decreasing also the mechanical properties.

Does anyone has a TTT or CCT diagram for EN 10088 - 1.4418?
Or does anyone know what kind of structure wil be formed?