gottemewrong
Structural
- Apr 22, 2007
- 9
hi pal's:
Im worry about my mortar toppings Which is 5mm is the thinner and about 15 mm the thicker, I have to overlay it in the old slab, I have to do it due to limited time. The thing is, it is prepared so the "thin pressed narra flooring" will be install by which will be hammered to stick well in the floor... I used plasterbond to achieve more adhision with my topping so it wont peel by the proccess... Any assuring idea is much appreciated..
Thanks alot;
Structureaddict
Im worry about my mortar toppings Which is 5mm is the thinner and about 15 mm the thicker, I have to overlay it in the old slab, I have to do it due to limited time. The thing is, it is prepared so the "thin pressed narra flooring" will be install by which will be hammered to stick well in the floor... I used plasterbond to achieve more adhision with my topping so it wont peel by the proccess... Any assuring idea is much appreciated..
Thanks alot;
Structureaddict