Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

thinning LPS3

Status
Not open for further replies.

Tmoose

Mechanical
Apr 12, 2003
5,626
I have 2 old jugs of LPS3 that are much thicker than I recall. I'd like to thin the LPS3 with some solvent that will evaporate harmlessly (to the LPS3) after application.

Suggestions?

thanks

Dan T
 
Replies continue below

Recommended for you

It's "thickish" anyway. I'm not sure about solvents. Can you pull up an MSDS sheet? Take small batches and try different solvents? Perhaps try LPS1 as a solvent?

Rod
 
Component
CASRN
Weight Percent

Aliphatic Hydrocarbon
64742-47-8
60 - 70%

Distillates Petroleum Hydrotreated Heavy Paraffinic
64742-54-7
5 - 10%

Propylene Glycol Mono-n-butyl Ether
5131-66-8
5 - 10%

Dipropylene Glycol Mono Butyl Ether
29911-28-2
1 - 5%

Light Mineral Spirits
64742-88-7/8052-41-3
1 - 5%

You could add a little more mineral spirits
 