Feb 14, 2022 #1 dlclarkii Structural Mar 29, 2005 37 0 0 US Pictures are of a 20T runway bearing on a 1914 multi wythe brick wall. Roof has been leaking. Upgrade in 1985 by supporting the center runways with new columns but the runway ends weren't reinforced. We failed the crane inspection.
Pictures are of a 20T runway bearing on a 1914 multi wythe brick wall. Roof has been leaking. Upgrade in 1985 by supporting the center runways with new columns but the runway ends weren't reinforced. We failed the crane inspection.
Feb 14, 2022 #2 miningman Mining Feb 26, 2003 957 0 0 CA cant say I'm surprised that it failed inspection Upvote 0 Downvote
Feb 14, 2022 #3 BAretired Structural Nov 16, 2008 10,839 0 36 CA Sandblasting is needed to see what section and weld metal is left. BA Upvote 0 Downvote
Feb 16, 2022 #4 kingnero Mechanical Aug 15, 2009 1,743 0 36 BE Love the upwards bent rail pic - haven't seen that being used instead of end stops. This must've taken enourmous amounts of heat and force. Is there any chance you could post a wider picture/overall view of the end of the rail? Thanks, a rail afficionado. Good luck with the crane though. Upvote 0 Downvote
Love the upwards bent rail pic - haven't seen that being used instead of end stops. This must've taken enourmous amounts of heat and force. Is there any chance you could post a wider picture/overall view of the end of the rail? Thanks, a rail afficionado. Good luck with the crane though.