Time dependant thermal properties of glass

Status
Not open for further replies.

28911982

Mechanical
Joined
Jul 21, 2003
Messages
5
Location
AU

Would anybody know where to look for time dependant thermal properties of glass?

I am interested in the conductivity and specific heat at 600 to 1200 degrees celcius.

Thanks.....
 
1) What is the composition of the glass?
2) Conductivity and specific heat are not generally considered time dependant thermal properties. However, some variation of parameters can occur during annealing of quenched specimens.
3) The Materials Science and Engineering Handbook, 3rd Edn., pp. 416-420 has data for the thermal conductivities of a number of glasses at various temperatures or over temperature ranges. The data were taken from Handbook of Glass Data, Part A and Part B, by O. V. Mazurin et al. (1983).
 
The thing for watch for with glasses is devitrification (crystallization). Devitrification is time dependent in cetain temperature windows for different glass compositins. There may be some little specific heat variation due to crystallization. In general, I would expect conductivity to increase with increasing crystallization (i. e. amorphous structures don't conduct heat well).

 
Does anyone here know of a good resource for analyzing glass breakage in the appliance industry? I am working on reducing breakage associated with TinO2 coated glass and am looking for a good resource.
 
here's some TC data for quartz in W/m/C

from

D.W. Lee and W.D. Kingery, J. American Ceramic Soc., v43, p594 (1960) and G.E. Childs, L.J. Ericks and R.L. Powell, NBS Monograph 131, p514,527 (1973)

1.0985e-001 -268.1
1.5081e-001 -258.1
1.9852e-001 -248.1
2.5175e-001 -238.1
3.0939e-001 -228.1
3.7036e-001 -218.1
4.3367e-001 -208.1
4.9842e-001 -198.1
5.6375e-001 -188.1
6.2890e-001 -178.1
6.9316e-001 -168.1
7.5592e-001 -158.1
8.1663e-001 -148.1
8.7481e-001 -138.1
9.3005e-001 -128.1
9.8202e-001 -118.1
1.0305e+000 -108.1
1.0752e+000 -98.1
1.1161e+000 -88.1
1.1532e+000 -78.1
1.1864e+000 -68.1
1.2160e+000 -58.1
1.2420e+000 -48.1
1.2647e+000 -38.1
1.2845e+000 -28.1
1.3017e+000 -18.1
1.3168e+000 -8.1
1.3304e+000 1.9
1.3495e+000 11.9
1.3711e+000 21.9
1.3909e+000 31.9
1.4091e+000 41.9
1.4258e+000 51.9
1.4413e+000 61.9
1.4556e+000 71.9
1.4688e+000 81.9
1.4812e+000 91.9
1.4928e+000 101.9
1.5037e+000 111.9
1.5141e+000 121.9
1.5241e+000 131.9
1.5337e+000 141.9
1.5430e+000 151.9
1.5522e+000 161.9
1.5613e+000 171.9
1.5705e+000 181.9
1.5796e+000 191.9
1.5889e+000 201.9
1.5984e+000 211.9
1.6082e+000 221.9
1.6182e+000 231.9
1.6286e+000 241.9
1.6394e+000 251.9
1.6507e+000 261.9
1.6624e+000 271.9
1.6746e+000 281.9
1.6874e+000 291.9
1.7008e+000 301.9
1.7147e+000 311.9
1.7292e+000 321.9
1.7444e+000 331.9
1.7602e+000 341.9
1.7767e+000 351.9
1.7939e+000 361.9
1.8117e+000 371.9
1.8302e+000 381.9
1.8494e+000 391.9
1.8692e+000 401.9
1.8898e+000 411.9
1.9111e+000 421.9
1.9330e+000 431.9
1.9557e+000 441.9
1.9790e+000 451.9
2.0030e+000 461.9
2.0277e+000 471.9
2.0530e+000 481.9
2.0790e+000 491.9
2.1056e+000 501.9
2.1329e+000 511.9
2.1609e+000 521.9
2.1895e+000 531.9
2.2187e+000 541.9
2.2486e+000 551.9
2.2790e+000 561.9
2.3101e+000 571.9
2.3419e+000 581.9
2.3742e+000 591.9
2.4072e+000 601.9
2.4408e+000 611.9
2.4750e+000 621.9
2.5099e+000 631.9
2.5454e+000 641.9
2.5816e+000 651.9
2.6185e+000 661.9
2.6560e+000 671.9
2.6942e+000 681.9
2.7332e+000 691.9
2.7729e+000 701.9
2.8135e+000 711.9
2.8548e+000 721.9
2.8969e+000 731.9
2.9400e+000 741.9
2.9839e+000 751.9
3.0289e+000 761.9
3.0748e+000 771.9
3.1219e+000 781.9
3.1700e+000 791.9
3.2194e+000 801.9
3.2700e+000 811.9
3.3220e+000 821.9
3.3754e+000 831.9
3.4302e+000 841.9
3.4867e+000 851.9
3.5448e+000 861.9
3.6048e+000 871.9
3.6666e+000 881.9
3.7304e+000 891.9
3.7963e+000 901.9
3.8645e+000 911.9
3.9350e+000 921.9
4.0080e+000 931.9
4.0837e+000 941.9
4.1622e+000 951.9
4.2436e+000 961.9
4.3282e+000 971.9
4.4160e+000 981.9
4.5074e+000 991.9
4.6024e+000 1001.9
4.7012e+000 1011.9
4.8041e+000 1021.9
4.9113e+000 1031.8
5.0230e+000 1041.8
5.1394e+000 1051.8
5.2608e+000 1061.8
5.3874e+000 1071.8
5.5194e+000 1081.8
5.6572e+000 1091.8
5.8010e+000 1101.8
5.9511e+000 1111.8
6.1077e+000 1121.8
6.3643e+000 1131.8
6.7573e+000 1141.8
7.2139e+000 1151.8
7.7391e+000 1161.8
8.3380e+000 1171.8
9.0157e+000 1181.8
9.7772e+000 1191.8
1.0450e+001 1199.8


here's some SH data for quartz in J/Kg/C

from

R.B. Scott, Cryogenic Engineering, Pub. D. van Nostrand Company, Inc., p329 (1962); C.F. Lucks, H.W. Deem and W.D. Wood, American Ceramic Society Bulletin, vol 39, p313 (1960); and L.H. van Vlack, Physcial Ceramics for Engineers, Addison-Wesley Publiching Co., p146 (1964)


2.6267e+001 -253.1
5.9424e+001 -243.1
9.2045e+001 -233.1
1.2413e+002 -223.1
1.5568e+002 -213.1
1.8669e+002 -203.1
2.1716e+002 -193.1
2.4710e+002 -183.1
2.7650e+002 -173.1
3.0537e+002 -163.1
3.3126e+002 -153.1
3.5508e+002 -143.1
3.7881e+002 -133.1
4.0241e+002 -123.1
4.2583e+002 -113.1
4.4903e+002 -103.1
4.7196e+002 -93.1
4.9459e+002 -83.1
5.1689e+002 -73.1
5.3883e+002 -63.1
5.6038e+002 -53.1
5.8152e+002 -43.1
6.0222e+002 -33.1
6.2246e+002 -23.1
6.4223e+002 -13.1
6.6151e+002 -3.1
6.8029e+002 6.9
6.9856e+002 16.9
7.1631e+002 26.9
7.3354e+002 36.9
7.5024e+002 46.9
7.6640e+002 56.9
7.8204e+002 66.9
7.9715e+002 76.9
8.1173e+002 86.9
8.2579e+002 96.9
8.3933e+002 106.9
8.5236e+002 116.9
8.6490e+002 126.9
8.7694e+002 136.9
8.8851e+002 146.9
8.9961e+002 156.9
9.1025e+002 166.9
9.2046e+002 176.9
9.3024e+002 186.9
9.3961e+002 196.9
9.4859e+002 206.9
9.5720e+002 216.9
9.6544e+002 226.9
9.7334e+002 236.9
9.8091e+002 246.9
9.8818e+002 256.9
9.9516e+002 266.9
1.0019e+003 276.9
1.0083e+003 286.9
1.0145e+003 296.9
1.0205e+003 306.9
1.0263e+003 316.9
1.0320e+003 326.9
1.0374e+003 336.9
1.0427e+003 346.9
1.0479e+003 356.9
1.0529e+003 366.9
1.0578e+003 376.9
1.0627e+003 386.9
1.0674e+003 396.9
1.0721e+003 406.9
1.0767e+003 416.9
1.0813e+003 426.9
1.0858e+003 436.9
1.0903e+003 446.9
1.0947e+003 456.9
1.0991e+003 466.9
1.1034e+003 476.9
1.1077e+003 486.9
1.1120e+003 496.9
1.1162e+003 506.9
1.1204e+003 516.9
1.1245e+003 526.9
1.1285e+003 536.9
1.1325e+003 546.9
1.1363e+003 556.9
1.1401e+003 566.9
1.1436e+003 576.9
1.1471e+003 586.9
1.1503e+003 596.9
1.1533e+003 606.9
1.1561e+003 616.9
1.1585e+003 626.9
1.1607e+003 636.9
1.1625e+003 646.9
1.1645e+003 656.9
1.1670e+003 666.9
1.1694e+003 676.9
1.1719e+003 686.9
1.1743e+003 696.9
1.1767e+003 706.9
1.1792e+003 716.9
1.1816e+003 726.9
1.1841e+003 736.9
1.1865e+003 746.9
1.1889e+003 756.9
1.1913e+003 766.9
1.1938e+003 776.9
1.1962e+003 786.9
1.1986e+003 796.9
1.2010e+003 806.9
1.2034e+003 816.9
1.2058e+003 826.9
1.2082e+003 836.9
1.2106e+003 846.9
1.2131e+003 856.9
1.2155e+003 866.9
1.2179e+003 876.9
1.2203e+003 886.9
1.2227e+003 896.9
1.2251e+003 906.9
1.2275e+003 916.9
1.2299e+003 926.9
1.2323e+003 936.9
1.2347e+003 946.9
1.2371e+003 956.9
1.2395e+003 966.9
1.2419e+003 976.9
1.2443e+003 986.9
1.2468e+003 996.9
1.2492e+003 1006.9
1.2516e+003 1016.9
1.2540e+003 1026.8
1.2564e+003 1036.8
1.2588e+003 1046.8
1.2613e+003 1056.8
1.2637e+003 1066.8
1.2661e+003 1076.8
1.2686e+003 1086.8
1.2710e+003 1096.8
1.2734e+003 1106.8
1.2759e+003 1116.8
1.2783e+003 1126.8
1.2808e+003 1136.8
1.2833e+003 1146.8
1.2857e+003 1156.8
1.2882e+003 1166.8
1.2907e+003 1176.8
1.2931e+003 1186.8
1.2956e+003 1196.8
1.2981e+003 1206.8
1.3006e+003 1216.8
1.3031e+003 1226.8
1.3056e+003 1236.8
1.3081e+003 1246.8
1.3106e+003 1256.8
1.3132e+003 1266.8
1.3157e+003 1276.8
1.3182e+003 1286.8
1.3208e+003 1296.8
1.3233e+003 1306.8
1.3259e+003 1316.8
1.3285e+003 1326.8
1.3311e+003 1336.8
1.3336e+003 1346.8
1.3362e+003 1356.8
1.3388e+003 1366.8
1.3415e+003 1376.8
1.3441e+003 1386.8
1.3467e+003 1396.8
1.3493e+003 1406.8
1.3520e+003 1416.8
1.3547e+003 1426.8
1.3573e+003 1436.8
1.3600e+003 1446.8
1.3627e+003 1456.8
1.3654e+003 1466.8
1.3681e+003 1476.8
1.3708e+003 1486.8
1.3735e+003 1496.8
1.3763e+003 1506.8
1.3790e+003 1516.8
1.3818e+003 1526.8
1.3846e+003 1536.8
1.3874e+003 1546.8
1.3902e+003 1556.8
1.3930e+003 1566.8
1.3958e+003 1576.8
1.3987e+003 1586.8
1.4015e+003 1596.8
1.4044e+003 1606.8
1.4073e+003 1616.8
1.4101e+003 1626.8
1.4131e+003 1636.8
1.4160e+003 1646.8
1.4189e+003 1656.8
1.4219e+003 1666.8
1.4248e+003 1676.8
1.4278e+003 1686.8
1.4308e+003 1696.8
1.4338e+003 1706.8
1.4368e+003 1716.8
1.4398e+003 1726.8
 