Does anyone have any experience with these tests being conducted in lieu of traditional Charpy impact tests?

Thanks
 
Replies continue below

Recommended for you

Technically, ASTM E143 is a test for shear modulus, not toughness. I assume that someone is referencing this method for a test setup that torsionally loads a cylindrical specimen until fracture? I have used torsion testing before, but not in lieu of charpy impact tests. Can you provide some additional detail on the application and why a torsion test is being specified?
 