Hello everyone,
I have a weird situation regarding some carbon steel welds (base material P265GH).
We installed a Waste Heat Boiler and after 3 weeks of operation some welds in the main steam line generate transversal cracks.
We replaced the pipe and the fittings and make new welds. After other 3 weeks, the welds started to crack again.
On this line there is a spray water injection. It's possible that the water can contain some substances that can affect the welds in such way that can generate transversal cracks?
Thanks!
I have a weird situation regarding some carbon steel welds (base material P265GH).
We installed a Waste Heat Boiler and after 3 weeks of operation some welds in the main steam line generate transversal cracks.
We replaced the pipe and the fittings and make new welds. After other 3 weeks, the welds started to crack again.
On this line there is a spray water injection. It's possible that the water can contain some substances that can affect the welds in such way that can generate transversal cracks?
Thanks!