Triflic acid corrosion; 160C ; Hast C276; 0.1% concentration

Status
Not open for further replies.

garyd78

Chemical
Oct 10, 2014
1
Does anyone know if triflic acid at 160C can be handled in Hast C276? 0.1% concentration. I saw a 2009 post from jfowler regarding catalytic level triflic in Hastelloy but no temp or concentration info nor the grade of hastelloy. thanks.
 