Trumpf cutting thick carbon on 5k

Status
Not open for further replies.
Replies continue below

Recommended for you

yes and it is possible but very poor edge quality and not worth the hassle. doesnt even cut well on a 6kw tanaka. i would use a plasma
 
it all depends on how much time you can afford to put into a part. dont get me wrong the machines will cut the parts you just have to have time to make the changes needed in the tech tables and from a production stand point it takes to long job shop type applications it is definitely worth the time
 