Hello to all,
we have a multitube heat exchanger (minimum center to center diameter: 14") with tube bundle according to UNS 39274 (superduplex) cold formed and solution annealing(U-bends and 12"). The tubesheet layout is square pitch (1") and the U-Bends have been formed according to triangular layout (15/16"). Due to long delivery date of new forged tubesheet (UNS 39274) or new tubes, we would like to repair the U-Bends safely. Please could you indicate any advice about Non-destructive and Destructive examination?
Thanks in advance