Hi all ,
we are in process of procuring tube bundle for our Kettle type S & T heat exchanger the following are the design parameters
Shell side tube side
corrosion allowance 0.125 0.125
design temp F 415 / 41 MDMT 500 / 41 MDMT
deisgn pressure psig 75 / FV 425 / FV
Test pressure psig 112.4 637.3
tube Moc SA 213 TP 316L
tube sheet MOC SA 516 Gr 70 + A 240 Gr 316l
code ASME Sec8 Div 1
Type BKU
Tema R
tube to tubesheet joint rolled and welded
Now vendor is suggest material A266 Gr 4 for tube sheet with clading with justification that forging is better then plate material due to high thickness (tube sheet thickness is 6.46" or 164 mm with 10 mm clad) .Is this change justifiable ?
Need guidance in this regards,
we are in process of procuring tube bundle for our Kettle type S & T heat exchanger the following are the design parameters
Shell side tube side
corrosion allowance 0.125 0.125
design temp F 415 / 41 MDMT 500 / 41 MDMT
deisgn pressure psig 75 / FV 425 / FV
Test pressure psig 112.4 637.3
tube Moc SA 213 TP 316L
tube sheet MOC SA 516 Gr 70 + A 240 Gr 316l
code ASME Sec8 Div 1
Type BKU
Tema R
tube to tubesheet joint rolled and welded
Now vendor is suggest material A266 Gr 4 for tube sheet with clading with justification that forging is better then plate material due to high thickness (tube sheet thickness is 6.46" or 164 mm with 10 mm clad) .Is this change justifiable ?
Need guidance in this regards,