ElCidCampeador
Mechanical
Hi,
I have a tubesheet Thk.120mm Mat. SA 266 Gr.2 and a tube D.25,4 Sp.2,22mm Mat. SA 179 welded to it as for a classic heat exchanger tubeesheet (fig. UW-20.1(d)).
Acc. to ASME VIII Div.1 design calculation tubesheet requires impact test @ MDMT but tube is exempted.
Question: does PQR of this weld require impact test too?
Thank you
I have a tubesheet Thk.120mm Mat. SA 266 Gr.2 and a tube D.25,4 Sp.2,22mm Mat. SA 179 welded to it as for a classic heat exchanger tubeesheet (fig. UW-20.1(d)).
Acc. to ASME VIII Div.1 design calculation tubesheet requires impact test @ MDMT but tube is exempted.
Question: does PQR of this weld require impact test too?
Thank you