19750412
Mechanical
- Feb 23, 2007
- 17
Dear All
I have two questions in the filed of interpretation of ASME. Now we design heat exchangers working in lethal services, in meaning of ASME VIII Div. 1 UW-2 (a). Acc. to data sheets, exchangers shall be BEM type and for that we chosen corner joint type “i” of fig. UW-13.2. Such solution is also necessary to keep inside diameter of shell and further to keep guarantee heat exchange. Of course this type of weld acc. to point UW-2 (a)(1)(b) & (c), shall be type 1 or 2 of table UW-12, but due to above explanation can not. And therefore, we decide to treat theses joints as butt welds and to make 100% of volumetric testing what in our eyes shall fulfill requirements of UW-2(a) concerning 100% RT of butt welds. As you can imaging for such joint it is impossible to perform RT testing, but instead of it, we decided to do ultrasonic test of 100% welds. And now my questions:
- can we stay with such design solution or we shall redesign exchangers?
- can we replace RT test by UT test based on UW-11(a)(7)?
For this exchangers our client specified tube’s material acc. to SA-213 UNS S31254, for which ASME II part D dose not specified allowable stresses in different temperatures. But this material is specified in ASME II part A. Dose anybody know whether any code case allow to use it in temperatures different from room temperature.
Thanks for help.
Arti
I have two questions in the filed of interpretation of ASME. Now we design heat exchangers working in lethal services, in meaning of ASME VIII Div. 1 UW-2 (a). Acc. to data sheets, exchangers shall be BEM type and for that we chosen corner joint type “i” of fig. UW-13.2. Such solution is also necessary to keep inside diameter of shell and further to keep guarantee heat exchange. Of course this type of weld acc. to point UW-2 (a)(1)(b) & (c), shall be type 1 or 2 of table UW-12, but due to above explanation can not. And therefore, we decide to treat theses joints as butt welds and to make 100% of volumetric testing what in our eyes shall fulfill requirements of UW-2(a) concerning 100% RT of butt welds. As you can imaging for such joint it is impossible to perform RT testing, but instead of it, we decided to do ultrasonic test of 100% welds. And now my questions:
- can we stay with such design solution or we shall redesign exchangers?
- can we replace RT test by UT test based on UW-11(a)(7)?
For this exchangers our client specified tube’s material acc. to SA-213 UNS S31254, for which ASME II part D dose not specified allowable stresses in different temperatures. But this material is specified in ASME II part A. Dose anybody know whether any code case allow to use it in temperatures different from room temperature.
Thanks for help.
Arti