Jul 2, 2015 #1 moe27 Industrial Oct 25, 2013 37 0 0 GB We have a welding procedure (FCAW) qualified on plate CJP to ASME sec IX for welding P1 groups 1 & 2 materials. Can a WPS qualified on plate CJP to ASME sec IX be used to weld tubular TYK joints? Regards, moe27
We have a welding procedure (FCAW) qualified on plate CJP to ASME sec IX for welding P1 groups 1 & 2 materials. Can a WPS qualified on plate CJP to ASME sec IX be used to weld tubular TYK joints? Regards, moe27
Jul 2, 2015 #2 DekDee Petroleum Mar 12, 2012 1,275 0 36 PH moe, Too many questions to be able to give you answers. Need more info, Cheers, DD Upvote 0 Downvote