Good Day Experts,
We have a Separator with following parameters
ASME VIII Div. 1
MDMT = -29 °C
Shell 516 Gr. 70 Impact = Yes
Forged Hub Impact SA 105N = Yes
Elbow 2” 11.07mm thk. SA 234 WPB Impact = Exempted
UCS-67 IMPACT TESTS OF WELDING PROCEDURES
(a) Welds made with filler metal shall be deposited using welding procedures qualified with impact testing in accordance with UG-84 when any of the following apply:
(1) when either base metal is required to be impact.
My question is regarding impact test of welding procedure for Forged Hub to Elbow weld. If I evaluate this weld, it gets exempted as governing thickness is 11.07mm. Do I still require a WPS with impact test for Forged Hub to Elbow weld to comply with UCS-67(a)(1)?
We have a Separator with following parameters
ASME VIII Div. 1
MDMT = -29 °C
Shell 516 Gr. 70 Impact = Yes
Forged Hub Impact SA 105N = Yes
Elbow 2” 11.07mm thk. SA 234 WPB Impact = Exempted
UCS-67 IMPACT TESTS OF WELDING PROCEDURES
(a) Welds made with filler metal shall be deposited using welding procedures qualified with impact testing in accordance with UG-84 when any of the following apply:
(1) when either base metal is required to be impact.
My question is regarding impact test of welding procedure for Forged Hub to Elbow weld. If I evaluate this weld, it gets exempted as governing thickness is 11.07mm. Do I still require a WPS with impact test for Forged Hub to Elbow weld to comply with UCS-67(a)(1)?