Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IDS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

UG-101, Proof Test per Displacement measurement for SS CF8M

Status
Not open for further replies.

Swap Material

Materials
Jan 28, 2022
1
Hi Expert,

Need your opinion, whether to proof test CF8M material by Displacement measurement?
I read "materials having a definitely determinable yield point"
By any other means can I do that?
 
Replies continue below

Recommended for you

For what reason? Is there a specification?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 