262
Is it correct UHA-44 does not require, altogether, the post cold forming heat treatment due to straining of duplex, martensitic and ferritic stainless steels?


Nasir
Welding Engineer
DESCON ENGINEERING LIMITED
PAKISTAN
 
Replies continue below

Recommended for you

UHA-44 only applies to cold forming or straining of austenitic alloys - see UHA-44 (a)1.
 
Dear MetEngr
So that means if straining and design tempearture exceeds the limits of Table UHA-44, heat treatment is not required for other than austenitic alloys, Right?