Bluecat46
Mechanical
- Oct 7, 2011
- 35
Gents
Hoping some one can enlighten me regarding Long range ultrasonic in Stainless steel.
I have spoken to one company they did not seam bothered about it testing 316L, but I spoke to another and I was informed that because of grain structure with in the 316L then the beam would bonce everywhere and not give a true picture.
Which one is right?
Thanks
Hoping some one can enlighten me regarding Long range ultrasonic in Stainless steel.
I have spoken to one company they did not seam bothered about it testing 316L, but I spoke to another and I was informed that because of grain structure with in the 316L then the beam would bonce everywhere and not give a true picture.
Which one is right?
Thanks