Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

unassigned material WPS

Status
Not open for further replies.

abangbikerz

Mechanical
Apr 3, 2012
68
we got issues with our client about our WPS to weld S275JR plate to SA516GR70 plate using WPS Pno 1 to P no 1 base metal range. As S275JR is unassigned material. I supposed welder qualification is not a problem because our welder qualified to weld using 7018 electrode. Welding process doesnt change.

Is that WPS is valid to use on the above base metal. Help me as im new guy and asme code is really complicated.
 
Replies continue below

Recommended for you

No, since this base material is unassigned (per Appendix D, Section IX), you must have a WPS that is qualified with this specific Grade for use.
 