Jun 11, 2014 #1 NX687 Mechanical Joined May 15, 2013 Messages 24 Location AU Found a paper that said this weld area has such low tensile that a test piece cannot be machined into a tensile test piece But we have it sealing at 1000c and Ultra high vacuum , just so long as you do not flex the welded area,, or it will crack
Found a paper that said this weld area has such low tensile that a test piece cannot be machined into a tensile test piece But we have it sealing at 1000c and Ultra high vacuum , just so long as you do not flex the welded area,, or it will crack
Jun 14, 2014 #2 EdStainless Materials Joined May 20, 2004 Messages 16,367 Location Waukesha WI USA Can use an explosive weld joint? Considering that the SS will have strength of a few 100psi at that temp you are going to have to very careful that you don't stress the joint anyway. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
Can use an explosive weld joint? Considering that the SS will have strength of a few 100psi at that temp you are going to have to very careful that you don't stress the joint anyway. = = = = = = = = = = = = = = = = = = = = Plymouth Tube