Apr 5, 2022 #1 Aswin_ad9 Mechanical Apr 5, 2022 1 0 0 AU We use a torsion rubber system with shore 70A rubber unit. Its quite stiff. want to soften it and increase the manufacturability
We use a torsion rubber system with shore 70A rubber unit. Its quite stiff. want to soften it and increase the manufacturability
Apr 5, 2022 #2 GregLocock Automotive Apr 10, 2001 23,129 2 38 Orbiting a small yellow star What is your static load on the wheel and what is the wheel rate? Cheers Greg Locock New here? Try reading these, they might help FAQ731-376 http://eng-tips.com/market.cfm? Upvote 0 Downvote