BAGW
Structural
- Jul 15, 2015
- 392
Hi,
Looking at some Europe equivalent grades for A992 and A36. Is it S355JR and S275JR? I assume the US standard V-notch testing is 27J at room temperature which grades JR satisfy.
When are the grades J0 and J2 used? Is it more of bridge application?
Thanks
Looking at some Europe equivalent grades for A992 and A36. Is it S355JR and S275JR? I assume the US standard V-notch testing is 27J at room temperature which grades JR satisfy.
When are the grades J0 and J2 used? Is it more of bridge application?
Thanks