Use ASTM-A312 TP316Ti and SA-182 F316TI for ASME section VIII Div-1

Status
Not open for further replies.

chonburi

Industrial
Jul 25, 2008
9
Dear member,
This two material is not in table UHA-23 and ref. to UHA-11(a). If user require to use this mat'l and vessel require U-Stamp. If you are Code certifica holder what we have to do?..please recommend sir. Thanks.
 
Replies continue below

Recommended for you

Unless there is an active Code Case for this material, it can't be used as pressure retaining material for Section VIII, Div 1 application.
 