I've tried Struers repliset and didn't much enjoy it.
Acetate remains my preference, although I've retired from field work. It requires some agile finger technique to get right, especially when bridging a big weld, so I would always prepare with one or two practice rounds. Pre-production tests if you will.
Good surface preparation and etching are the keys.