Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

varying thickness of RAFT slabs

Status
Not open for further replies.

brick2020

Structural
Jul 5, 2013
15
Hi All...

I have a raft under a building that is 1200mm.. and also a portion of th ebuilding where the raft os 750mm thick.
How should i joing the raft with varying thickness.. shoudl i taper the 1200mm raft to 750 gradually.. or is it ok to have sudden drop from 122-750?

I have cheacked , and there is no stress concentratio n near the edges.

any standard details in ACI?


 