How do you figure out how much expansion you will get from a masonry veneer?
I would suspect that you would calculate the moisture expansion using the coefficient of moisture expansion for clay masonry and add that to the calculated thermal expansion using coefficient of thermal expansion for clay masonry.
Therefore, for a 25’ tall veneer wall in an area with a 50 degree temperature swing you would get 25*12*3*10^-4+25*12*50*4*10^-6 = 0.15 inches.
Is this correct?