May 17, 2004 #1 hyperen Aerospace Apr 20, 2004 9 0 0 GR Dear all, my .f06 file contains the element and plies that have failed using the TSAI WU criterion. However my model has more than 3000 elements. How can I import those results containing the failed elements so I can group them and viwe them? Cheers hyperen
Dear all, my .f06 file contains the element and plies that have failed using the TSAI WU criterion. However my model has more than 3000 elements. How can I import those results containing the failed elements so I can group them and viwe them? Cheers hyperen
Aug 6, 2004 #2 macrohard New member Aug 6, 2004 1 0 0 DE Utilitites>Results>Read MSC.N Failure indices. Do it before attaching xdb file. Mit freundlichen Grüßen Macrohard Upvote 0 Downvote