SuG89
Structural
- Aug 10, 2014
- 118
Hello,
I am a beginner in Femap. I have defined the following stress vs strain curve for a steel material:
Strain Stress
0 0
0.002 (0.2% ) 300 MPa
0.2 (20% ) 500 MPa
I had expected that the von Mises stress results would in any case be less than (or equal to) 500 MPa for the above definition which is not the case in my model.
On another public forum, I had posted the same query and got a response from a very advanced Femap user that this could be due to extrapolation of stresses from the integration points to the grids or element centroid. He suggested to look at gauss point stresses rather than the nodal values. Could anyone tell me steps to look at the Gauss point stresses in Femap?
Best regards,
Su
I am a beginner in Femap. I have defined the following stress vs strain curve for a steel material:
Strain Stress
0 0
0.002 (0.2% ) 300 MPa
0.2 (20% ) 500 MPa
I had expected that the von Mises stress results would in any case be less than (or equal to) 500 MPa for the above definition which is not the case in my model.
On another public forum, I had posted the same query and got a response from a very advanced Femap user that this could be due to extrapolation of stresses from the integration points to the grids or element centroid. He suggested to look at gauss point stresses rather than the nodal values. Could anyone tell me steps to look at the Gauss point stresses in Femap?
Best regards,
Su