Hi Folks
I need your help, I want to weaken some parts in a
steel pipe (Failure phenomenon which is related
directly to residual stress termed “stress corrosion
cracking”. This occurs in metals which are subjected
to corrosive environments whilst stressed),
The best way for that will be through controlling the
residual stresses. Can any body tell me how to control
residual stresses in ABAQUS.
I searched in the Documentation, but I found just one
relevant sentence talking about The relief of residual
stresses through creep.
I need your help, I want to weaken some parts in a
steel pipe (Failure phenomenon which is related
directly to residual stress termed “stress corrosion
cracking”. This occurs in metals which are subjected
to corrosive environments whilst stressed),
The best way for that will be through controlling the
residual stresses. Can any body tell me how to control
residual stresses in ABAQUS.
I searched in the Documentation, but I found just one
relevant sentence talking about The relief of residual
stresses through creep.