How do I evaluate the nominal base metal stress at the toe of a fillet weld? The nominal stress is 19.2ksi and less than the plate's yield strength (30ksi), however I know a localized stress concentration (i.e. weld toe) exists at this location. I have searched a number of codes (AWS, IIW, AISC, etc.) and I can't find any mention of stress concentration under static loading conditions. Are these stress concentrations to be ignored, or is it cooked into the code?
For AWS D1.1, should I convert the nominal stress (Von Mises) to maximum shear stress and compare that to 0.4 * yield (12ksi)?
Thanks
For AWS D1.1, should I convert the nominal stress (Von Mises) to maximum shear stress and compare that to 0.4 * yield (12ksi)?